Esab OK 385 Tig rods diam. 2.4 cf. of KG. 5
OK Tigrod 385
Stainless steel rod for TIG welding of 20Cr-25Ni-4.5Mo-1.5Cu (904 L) steels. Good resistance
to stress corrosion and intergranular corrosion, excellent resistance to attack by non-oxidizing acids.
Pitting and crevice corrosion resistance are also better than typical 18Cr-8Ni-Mo steel deposits.
(edit with the Customer Reassurance module)
(edit with the Customer Reassurance module)
(edit with the Customer Reassurance module)
Specifications
Classifications EN ISO 14343-A : W 20 25 5 Cu L
SFA/AWS A5.9 : ER385
Approvals NAKS/HAKC : 2.4mm
VdTÜV : 05444
Approvals are based on factory location. Please contact ESAB for more information.
Alloy type Fully austenitic (20 % Cr - 25 % Ni - 5 % Mo - 1.5 % Cu - Low C)
Typical tensile properties
State Yield strength Tensile strength Stretching
As welded 340 MPa
( 49 ksi )
540 MPa
( 78 ksi )
37%
Charpy V-notch test properties
State Test temperature Tenacity value
As welded 20 °C ( 68 °F ) 120 J ( 89 ft-lb )
Weld Metal Analysis
C Yes Mn Cr No Mo Who N
Typical Wire Composition %
0.01 0.4 1.7 20.0 25.0 4.4 1.5 0.05